反応 #4121324
関連文献 (1)
openreactiondata ↗doi:10.1039/C8SC04228D
反応条件: temp:0.00; pressure:0.00; stir:
ソース ID: ord-1d5659243c534ce4afc5bfe5db6dbfda表示可能な構造データがありません
CCCCCCC1CO1製品情報
2-hexyloxirane (CAS 26637-94-5) product identity, structure identifiers and related reaction data for chemical intermediate research and sourcing review.
想定用途
専門的研究・工業用途限定
データベース ID 18126
安全上の注意
For professional research and industrial use only. Review the supplier safety data sheet before handling.
合成データ
12 反応 · 12 文献
反応条件: temp:0.00; pressure:0.00; stir:
ソース ID: ord-1d5659243c534ce4afc5bfe5db6dbfda反応条件: temp:0.00; pressure:0.00; stir:
ソース ID: ord-ba302647a82c4972ad4ec3338f9c5347反応条件: temp:0.00; pressure:0.00; stir:
ソース ID: ord-c78767dc20a14bd6a97e5fc4dac8562c反応条件: temp:0.00; pressure:0.00; stir:
ソース ID: ord-9212d22bbe5c45e2b5754d48d55028b7反応条件: temp:0.00; pressure:0.00; stir:
ソース ID: ord-3af7404251e74d8f84a69d3908d3108e反応条件: temp:0.00; pressure:0.00; stir:
ソース ID: ord-af2dc4f35da84a85b07e4984e86da141反応条件: temp:0.00; pressure:0.00; stir:
ソース ID: ord-bcf7d5a0f5c54e6d85ef1dcfc57f8927反応条件: temp:130.01; pressure:0.00; stir:; See reaction.notes.procedure_details.
実験手順: The epoxyoctane hydrophobic dense star polymer described in Example 10 (0.1 g) was dissolved in a mixture of 1 g of octene and 19 g of styrene. Azobisisobutyronitrile (0.15 g) was added and the resulting solution was heated at 100° C. for 0.5 day and 130° C. for 1 day to give a solid polymer. to give a solid polymer
ソース ID: ord-80b85be3feb64a0a8bdcd101aab0a634反応条件: temp:130.01; pressure:0.00; stir:; See reaction.notes.procedure_details.
実験手順: The epoxyoctane hydrophobic dense star polymer described in Example 10 (0.1 g) was dissolved in a mixture of 1 g of octene and 19 g of styrene. Azobisisobutyronitrile (0.15 g) was added and the resulting solution was heated at 100° C. for 0.5 day and 130° C. for 1 day to give a solid polymer. to give a solid polymer
ソース ID: ord-80b85be3feb64a0a8bdcd101aab0a634反応条件: temp:130.01; pressure:0.00; stir:; See reaction.notes.procedure_details.
実験手順: The epoxyoctane hydrophobic dense star polymer described in Example 10 (0.1 g) was dissolved in a mixture of 1 g of octene and 19 g of styrene. Azobisisobutyronitrile (0.15 g) was added and the resulting solution was heated at 100° C. for 0.5 day and 130° C. for 1 day to give a solid polymer. to give a solid polymer
ソース ID: ord-492aad0da9644f339a31f3739afdd844反応条件: temp:130.01; pressure:0.00; stir:; See reaction.notes.procedure_details.
実験手順: The epoxyoctane hydrophobic dense star polymer described in Example 10 (0.1 g) was dissolved in a mixture of 1 g of octene and 19 g of styrene. Azobisisobutyronitrile (0.15 g) was added and the resulting solution was heated at 100° C. for 0.5 day and 130° C. for 1 day to give a solid polymer. to give a solid polymer
ソース ID: ord-492aad0da9644f339a31f3739afdd844反応条件: temp:130.01; pressure:0.00; stir:; See reaction.notes.procedure_details.
実験手順: The epoxyoctane hydrophobic dense star polymer described in Example 10 (0.1 g) was dissolved in a mixture of 1 g of octene and 19 g of styrene. Azobisisobutyronitrile (0.15 g) was added and the resulting solution was heated at 100° C. for 0.5 day and 130° C. for 1 day to give a solid polymer. to give a solid polymer
ソース ID: ord-377fa74e98844954b99fdc6abfdde6b9PubChem References
化合物の公開データベース記録に掲載された情報源です。